徐红勇, 王瑾, 聂盼, 吉华, 洪晓祥, 张阳阳. 搅拌摩擦点焊工艺参数对接头组织及力学性能的影响[J]. 焊接, 2020, (8): 33-38,63. DOI: 10.12073/j.hj.20200730001
引用本文: 徐红勇, 王瑾, 聂盼, 吉华, 洪晓祥, 张阳阳. 搅拌摩擦点焊工艺参数对接头组织及力学性能的影响[J]. 焊接, 2020, (8): 33-38,63. DOI: 10.12073/j.hj.20200730001
XU Hongyong, WANG Jin, NIE Pan, JI Hua, HONG Xiaoxiang, ZHANG Yangyang. Effect of parameters on microstructure and mechanical properties of friction stir spot welded joint[J]. WELDING & JOINING, 2020, (8): 33-38,63. DOI: 10.12073/j.hj.20200730001
Citation: XU Hongyong, WANG Jin, NIE Pan, JI Hua, HONG Xiaoxiang, ZHANG Yangyang. Effect of parameters on microstructure and mechanical properties of friction stir spot welded joint[J]. WELDING & JOINING, 2020, (8): 33-38,63. DOI: 10.12073/j.hj.20200730001

搅拌摩擦点焊工艺参数对接头组织及力学性能的影响

Effect of parameters on microstructure and mechanical properties of friction stir spot welded joint

  • 摘要: 采用回填式搅拌摩擦点焊技术制备1.0 mm厚6016-T4铝合金点焊接头,并通过正交试验法对其表面成形、剪切拉伸、十字拉伸和显微硬度进行分析,探究焊接工艺参数对6016-T4铝合金点焊接头组织及力学性能的影响。结果表明,焊接时间4.5 s、旋转速度1 600 r/min、下扎深度1.4 mm为最佳焊接工艺参数,接头剪切拉伸力、十字拉伸力分别为4.02 kN与1.32 kN;中间部位的搅拌针作用区硬度较为均匀,硬度值高于母材区;焊点接头在剥离试验过程中均未出现松动,说明焊点牢固,质量良好。

     

    Abstract: Refill friction stir spot welding joint of a 1.0 mm thickness 6016-T4 aluminum alloy was prepared by different parameters.The comprehensive properties of 6016-T4 aluminum alloy joint by different parameters was studied through the analysis of its surface formation,shear tensile,crossing tensile and micro-hardness by using orthogonal test.The results show that the optimum parameters are with the welding time of 4.5 s,the rotation speed of 1 600 rpm and the depth of 1.4 mm.The shear tensile force and cross tensile strength of the joint are respectively 4.02 kN and 1.32 kN.The micro-hardness of the action area of the pin is more uniform,and the micro-hardness value is higher than that of the base metal area.The joints do not show any looseness during the peeling tensile test,indicating that the joints are firm and qualified.

     

/